Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Thermoplastic Polyurethane Elastomer (TPU) Testing: Standards, Methods, and Applications

Thermoplastic polyurethane elastomer (TPU) testing is essential for verifying the mechanical performance, thermal stability, chemical composition, and regulatory compliance of this versatile engineering material. Accredited third-party laboratories apply internationally recognized standards from ISO, ASTM, IEC, and GB to characterize TPU resins, films, and finished products used in footwear, cable, automotive, and medical applications. This article provides a comprehensive overview of TPU sample types, testing items, test methods, and industry applications.

Technical Overview

Thermoplastic polyurethane elastomer (TPU) is a linear segmented block copolymer consisting of rigid hard segments, formed from diisocyanates and chain extenders, and flexible soft segments, derived from polyether or polyester polyols. This unique molecular architecture gives TPU an exceptional combination of high elasticity, abrasion resistance, tear strength, oil and grease resistance, and a broad hardness range spanning approximately Shore 60A to Shore 85D. Because TPU is melt-processable, it can be injection molded, extruded, calendered, blown into films, or used as a hot-melt adhesive base.

The performance of TPU depends heavily on the ratio of hard to soft segments, the type of polyol backbone, additives, and processing conditions. Systematic testing is therefore required for incoming material inspection, supplier qualification, batch-to-batch quality control, failure analysis, reverse engineering, and regulatory compliance. Accredited third-party laboratories typically conduct TPU testing under ISO/IEC 17025 quality management systems, applying standardized methods published by ISO, ASTM, IEC, UL, and national bodies such as GB standards in China.

Testing Samples

TPU Resins, Granules, and Powders

Pelletized or powdered TPU materials are tested in their raw state for melt flow rate, moisture content, density, intrinsic viscosity, molecular weight distribution, and ash content. These fundamental parameters determine processability and are often the first checkpoint in incoming inspection for injection molding and extrusion operations.

TPU Films and Sheets

Cast, blown, or calendered TPU films are evaluated for tensile strength, elongation at break, tear resistance, puncture resistance, optical transparency, haze, thickness uniformity, and bonding performance in laminated textile composites.

Extruded and Molded Products

Tubes, hoses, seals, gaskets, diaphragms, belts, casters, and injection-molded parts are tested for mechanical properties, compression set, hydrolysis resistance, and dimensional stability. Where finished parts cannot be used directly, test plaques are prepared from the material by compression or injection molding.

Cables and Wires with TPU Jackets

TPU-sheathed cables are assessed for insulation and sheath mechanical properties before and after aging, flame retardancy, and resistance to oils, fuels, and abrasion in accordance with IEC, UL, and EN cable standards.

Adhesives, Coatings, and 3D Printing Filaments

TPU-based hot-melt adhesives, coating powders, and additive manufacturing filaments are characterized for NCO content, hydroxyl value, softening point, melt viscosity, moisture level, and printability-related flow behavior.

Testing Items

Physical and Mechanical Properties

  • Shore A / Shore D hardness
  • Tensile strength, elongation at break, and 100% / 300% modulus
  • Tear strength (trouser, angle, and crescent methods)
  • Abrasion resistance (rotating cylindrical drum method)
  • Compression set and stress relaxation
  • Flex fatigue, cut growth, and dynamic mechanical properties (DMA)
  • Density, impact resistance, and bounce/rebound resilience

Thermal Properties

  • Melting point, melting enthalpy, and glass transition temperature by DSC
  • Thermogravimetric analysis (TGA) for decomposition and filler content
  • Vicat softening temperature and heat deflection temperature (HDT)
  • Low-temperature brittleness, Gehman stiffness, and temperature retraction (TR)
  • Thermal aging and heat resistance after oven exposure
  • Melt mass-flow rate (MFR) and melt volume-flow rate (MVR)

Chemical and Molecular Characterization

  • FTIR spectroscopy for chemical structure identification and polyol type differentiation
  • Isocyanate (NCO) group content by titration
  • Hydroxyl value and acid value of raw materials
  • Moisture content by Karl Fischer titration
  • Molecular weight and molecular weight distribution by GPC/SEC
  • Ash content and elemental composition by ICP-OES or ICP-MS

Electrical Properties

  • Volume and surface resistivity
  • Dielectric strength (electric strength)
  • Relative permittivity and dissipation factor

Flame Retardancy

  • UL 94 horizontal and vertical burning classification (HB, V-2, V-1, V-0)
  • Limiting oxygen index (LOI)
  • Glow-wire flammability index (GWFI) and glow-wire ignition temperature (GWIT)

Environmental Durability and Aging

  • Xenon-arc and fluorescent UV weathering with color change and property retention
  • Hydrolysis resistance under elevated temperature and humidity
  • Ozone resistance
  • Resistance to oils, fuels, solvents, acids, alkalis, and sweat by immersion testing
  • Yellowing and light stability for transparent or light-colored grades

Restricted Substances and Regulatory Compliance

  • RoHS heavy metals (lead, cadmium, mercury, hexavalent chromium) per IEC 62321
  • REACH SVHC screening and phthalate plasticizer content
  • Polycyclic aromatic hydrocarbons (PAHs) and halogen content
  • Food-contact and medical-grade migration testing where applicable

Testing Methods

Representative international and national standards commonly applied to TPU testing are summarized below. Specimens are typically conditioned at 23 °C and 50% relative humidity in accordance with ISO 291 or GB/T 2918 before mechanical testing, and test plaques are prepared by compression or injection molding per ISO 20753 or ASTM D4703.

  • Density: ISO 1183-1, ASTM D792, GB/T 1033.1 (immersion method)
  • Shore hardness: ISO 7619-1, ASTM D2240, GB/T 531.1
  • Tensile properties: ISO 37, ASTM D412, GB/T 528
  • Tear strength: ISO 34-1, ASTM D624, GB/T 529
  • Abrasion resistance: ISO 4649, ASTM D5963, GB/T 9867
  • Compression set: ISO 815-1, ASTM D395, GB/T 7759.1
  • Melt flow rate: ISO 1133-1, ASTM D1238, GB/T 3682.1
  • DSC thermal analysis: ISO 11357, ASTM D3418, GB/T 19466
  • Thermogravimetric analysis: ISO 11358, ASTM E1131
  • Vicat softening point: ISO 306, ASTM D1525, GB/T 1633
  • Heat deflection temperature: ISO 75-1/-2, ASTM D648, GB/T 1634
  • Low-temperature brittleness: ASTM D746, GB/T 15256
  • NCO content: ASTM D2572 titration method
  • Hydroxyl value: ASTM D4274
  • Water content: ISO 15512, ASTM D4019 (Karl Fischer)
  • Molecular weight by GPC: ISO 16014, ASTM D5296
  • Chemical resistance immersion: ISO 175, ASTM D543, GB/T 11547
  • Artificial weathering: ISO 4892-2/-3, ASTM G155, ASTM G154, GB/T 16422
  • Ozone resistance: ISO 1431-1, GB/T 7762
  • Dielectric strength: IEC 60243-1, GB/T 1408.1
  • Resistivity: IEC 62631-3-1/-2, GB/T 1410
  • Flammability: UL 94, IEC 60695-11-10, GB/T 2408
  • Limiting oxygen index: ISO 4589-2, ASTM D2863, GB/T 2406.2

Method selection depends on the intended application, the product form, and the specification invoked by the customer or end-use regulation. For durability studies, mechanical properties such as tensile strength and elongation are typically re-measured after aging exposure, and results are reported as percentage retention relative to unaged control specimens.

Applications

TPU testing supports a wide range of downstream industries where material reliability is critical:

  • Footwear: outsoles, midsole cushioning, toe caps, and transparent upper films requiring abrasion, flex, and yellowing resistance verification
  • Wires and cables: jacketing for robotics, drag-chain, mining, and renewable-energy cables demanding oil resistance and flame compliance
  • Automotive: seals, gaiters, airbag covers, interior skins, and paint-protection films requiring heat aging and chemical resistance data
  • Medical devices: catheter tubing, wound-dressing films, and hospital bedding needing biocompatibility screening and hydrolysis stability
  • Consumer electronics: protective cases, wearable straps, and cable accessories requiring wear and cosmetic durability testing
  • Industrial components: hoses, conveyor belts, drive belts, seals, and casters subject to dynamic fatigue and fluid exposure
  • Textiles: waterproof breathable TPU membranes and coated fabrics evaluated for hydrostatic resistance and laminated strength
  • Additive manufacturing: flexible filaments and powders verified for melt flow, moisture, and mechanical consistency

FAQ

Why is TPU testing important?

TPU properties vary significantly with formulation, and subtle changes in hard-segment content, moisture level, or processing can cause large shifts in hardness, tensile performance, and durability. Testing verifies that materials meet design specifications, supports supplier comparison, prevents field failures, and demonstrates compliance with regulatory requirements.

Which hardness scale should be used for TPU?

Soft TPU grades below approximately Shore 90A are measured on the Shore A scale, while harder grades are measured on the Shore D scale. The two scales overlap in the Shore 90A to 60D region, and specifications should clearly indicate which scale and standard apply.

What sample quantity is needed for a full test program?

Requirements vary by method, but a typical full mechanical and thermal characterization of pellets or plaques generally requires several hundred grams of material, while individual tests such as hardness or FTIR identification can be completed on small coupons or a few grams of resin.

How is hydrolysis resistance evaluated?

Standard practice involves accelerated exposure to hot water or elevated temperature and humidity, for example 85 °C and 85% relative humidity, followed by retesting of tensile strength and elongation. Retention values above a defined threshold, commonly 70% to 80%, indicate acceptable long-term hydrolytic stability for the intended service environment.

Can TPU be distinguished from other thermoplastic elastomers analytically?

Yes. FTIR spectroscopy identifies characteristic urethane carbonyl and N–H absorption bands, and it can further distinguish polyether-type from polyester-type TPU. Combined with DSC melting behavior, density, and elemental analysis, TPU can be reliably differentiated from TPE-S, TPO, TPV, and TPC materials.

How long does TPU testing take?

Routine physical and thermal tests are typically completed within five to ten working days after sample conditioning. Programs involving aging, weathering, or hydrolysis exposure require additional time proportional to the exposure duration specified in the applicable standard or customer protocol.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time