GB 8624 combustion testing is the mandatory Chinese national standard framework for classifying the burning behavior of building materials and products into fire performance Grades A, B1, B2 and B3. This technical guide explains the classification system, laboratory test methods, specimen requirements, key measurement parameters and typical applications. It is intended for manufacturers, architects, fire safety engineers and compliance professionals supplying materials to the Chinese construction market.
Technical Overview
GB 8624, titled "Classification of burning behavior for building materials and products," is a mandatory national standard that defines how the fire performance of construction materials is tested and graded in China. The current edition, GB 8624-2012, replaced the 2006 edition and has been in effect since June 1, 2013. The standard applies to flat building products, linear pipe insulation products and floor coverings used in building construction and interior decoration.
GB 8624-2012 is methodologically harmonized with EN 13501-1, the European fire classification standard, sharing the same core test methods and measurement parameters. However, it retains the traditional Chinese grade designations A, B1, B2 and B3 that are referenced by national fire design codes, and it adds a smoke toxicity classification that is unique to the Chinese system.
Classification Grades
Combustion performance is divided into four major grades containing seven sub-levels:
- Grade A (sub-classes A1 and A2): non-combustible materials that make no or only a very limited contribution to fire.
- Grade B1 (sub-classes B and C): flame-retardant materials with a limited contribution to fire growth.
- Grade B2 (sub-classes D and E): combustible materials that make an acceptable but notable contribution to fire.
- Grade B3 (class F): readily combustible materials that fail to meet the requirements of the higher grades.
In addition to the fire growth grade, a full classification carries supplementary notations for smoke production (s1, s2, s3), flaming droplets and particles (d0, d1, d2) and smoke production toxicity (t0, t1, t2). A complete result is therefore expressed, for example, as "B1 (B, s1, d0, t1)".
Testing Samples
Specimen configuration and quantity depend on the product form and the target classification. All specimens must be representative of normal production and tested in their end-use configuration, including any substrate, air gap, joint or surface treatment that will exist in real installation. Specimens are conditioned before testing at 23 ± 2 °C and 50 ± 5 % relative humidity for the period specified by each method.
Flat Products: Boards, Panels and Sheets
The single burning item test requires three complete specimen sets, each consisting of a long wing of 1500 mm × 500 mm and a short wing of 1500 mm × 1000 mm mounted at right angles in a corner configuration. The small flame ignitability test uses strips of 250 mm × 90 mm, typically six or more per configuration. Non-combustibility testing requires five cylindrical specimens of 45 mm diameter and 50 mm height, and the heat of combustion test requires approximately 50 g of material in powdered or cut form.
Thermal Insulation Materials
Rigid boards, flexible blankets, foam products and pipe-section insulation are tested according to their intended application. Homogeneous products are evaluated as a single material, while non-homogeneous or multi-layer products must be assessed component by component, including facings, adhesives and coatings, because each layer contributes to the classification result.
Wall, Ceiling and Decorative Finishes
Coatings, wallpapers, laminates, films and decorative textiles must be applied to a representative substrate identical to the end-use installation, since the substrate strongly influences ignition and flame spread behavior. Testing the material alone, without its substrate, does not produce a valid classification.
Floor Coverings
Resilient flooring, carpet, wood flooring and laminates follow a dedicated classification route based on the radiant panel test, using specimens of approximately 1050 mm × 230 mm, combined with the small flame test. The reported parameter is the critical heat flux at which flame spread extinguishes.
Testing Items
Depending on the classification level sought, the following parameters are measured during a GB 8624 evaluation:
- Furnace temperature rise, mass loss and duration of sustained flaming, from the non-combustibility test (GB/T 5464).
- Gross heat of combustion (PCS) of the finished product and of each individual component (GB/T 14402).
- Fire growth rate index (FIGRA), total heat release within 600 seconds (THR600s) and lateral flame spread (LFS), from the single burning item test (GB/T 20284).
- Smoke growth rate (SMOGRA) and total smoke production rate within 600 seconds, used for the s-classification.
- Occurrence and duration of flaming droplets and particles, used for the d-classification.
- Ignitability under a small flame source: flame spread distance, afterflame time and ignition of filter paper by falling droplets (GB/T 8626).
- Smoke production toxicity, based on the yields of toxic gases such as carbon monoxide, hydrogen cyanide and hydrogen chloride, graded into safety levels (GB/T 20285).
- Critical heat flux at extinguishment for floor coverings (GB/T 11785).
For products other than floorings, the principal quantitative criteria include FIGRA no greater than 120 W/s and THR600s no greater than 7.5 MJ for sub-class B, FIGRA no greater than 250 W/s and THR600s no greater than 15 MJ for sub-class C, and FIGRA no greater than 750 W/s for sub-class D.
Testing Methods
Non-Combustibility Test: GB/T 5464 (equivalent to ISO 1182)
Five cylindrical specimens are inserted one at a time into a tubular furnace stabilized at 750 °C and held for 30 minutes. Temperature rise inside the furnace, specimen mass loss and the duration of any sustained flaming are recorded. To support a Grade A classification, temperature rise must not exceed 30 °C, mass loss must not exceed 50 % and no significant sustained flaming may occur.
Gross Heat of Combustion: GB/T 14402 (equivalent to ISO 1716)
A bomb calorimeter measures the total potential heat release of small test portions of the product and, for non-homogeneous products, of each component layer. Sub-class A1 requires a gross heat of combustion of no more than 2.0 MJ/kg for homogeneous products, with component-specific limits applied to layered constructions. This method establishes the maximum energy theoretically available from the material.
Single Burning Item Test: GB/T 20284 (based on EN 13823)
The specimen wings are mounted vertically in a corner on a trolley and exposed to a nominally 30 kW gas burner that simulates a single burning item, such as a wastepaper basket, in a room corner. Exhaust gases are analyzed to derive heat release rate and smoke production, while the specimen is observed for lateral flame spread and flaming droplets. This test generates FIGRA, THR600s, SMOGRA and the droplet classification, and it is the core method for sub-classes B, C and D.
Small Flame Ignitability: GB/T 8626 (equivalent to ISO 11925-2)
Vertical specimens of 250 mm × 90 mm are exposed to a small propane flame applied either for 15 seconds (sub-class E route) or 30 seconds (sub-class B, C and D route). The specimen passes if the flame tip does not reach the 150 mm gauge line within the criterion time, if afterflame time is within limits, and if falling droplets do not ignite filter paper placed beneath the specimen.
Smoke Production Toxicity: GB/T 20285
Specimens are decomposed in a flow-through furnace under defined temperature and ventilation conditions, and the concentrations of hazardous gases in the effluent are quantified. Results are graded into safety levels AQ1 and AQ2 and a danger level, which map to the supplementary notations t0, t1 and t2 respectively. This requirement reflects the Chinese regulatory emphasis on smoke hazard, since smoke inhalation is a leading cause of fire casualties.
Radiant Panel Test for Floorings: GB/T 11785
A horizontal flooring specimen is exposed to an inclined radiant panel that creates a gradient of heat flux along its length. After pilot ignition, the distance at which flame spread stops is converted into a critical heat flux value, which determines the fire growth grade of the floor covering.
Applications
GB 8624 classification is a statutory input to building design, fire review and material acceptance across China, and test reports from accredited third-party laboratories are routinely required in the following contexts:
- Interior wall and ceiling finishes in high-rise buildings, hospitals, schools, hotels, shopping malls and places of assembly, where fire design codes require Grade B1 or higher, and Grade A for specific elements and escape routes.
- External wall insulation systems, curtain wall components and facade panels.
- Thermal insulation for air ducts, piping and plant rooms.
- Metro and railway station fit-out materials and tunnel lining products.
- Product certification, public tender submissions and market entry documentation for manufacturers supplying the Chinese construction sector.
FAQ
What is the current version of GB 8624?
The current version is GB 8624-2012, which has been mandatory since June 1, 2013. All new classifications should be issued under this edition.
How does GB 8624-2012 differ from the 2006 edition?
The 2012 edition restored the familiar A, B1, B2 and B3 grade names, which the 2006 edition had replaced with the A1-to-F nomenclature, and introduced the smoke toxicity t-classification under GB/T 20285. The underlying test methods were retained and further aligned with EN 13501-1.
Is GB 8624 equivalent to the European Euroclass system?
The test methods and parameters are closely harmonized with EN 13501-1, so data can often be correlated between the two systems. However, the grade nomenclature differs, and the Chinese standard adds a smoke toxicity requirement that has no direct counterpart in the European classification.
How many samples are required for a full GB 8624 evaluation?
A typical program consumes five cylinders for the non-combustibility test, approximately 50 g of powder for heat of combustion, three complete SBI specimen sets, six or more small-flame strips, and additional material for toxicity testing. Accredited third-party laboratories normally request surplus material to allow repeat tests in case of borderline results.
How long does GB 8624 testing take?
A standard single-product program generally takes two to four weeks, including conditioning and report issuance. Multi-layer or composite products requiring component-by-component heat of combustion analysis may take longer.
Which grade do common materials achieve?
Mineral wool and similar inorganic products typically reach A1 or A2, gypsum-based boards commonly achieve A2, flame-retardant treated wood and engineered plastics are classified B1, and untreated plastics and ordinary textiles frequently fall into B2 or B3. The required grade depends on the application and occupancy type defined by national fire design codes.
Why Choose ZKGX?
- State-of-the-art analytical equipment
- Highly qualified scientific team
- Fast turnaround time
- Competitive pricing