Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Carburized Layer Hardness Gradient Measurement – Effective Case Depth Testing and Hardness Profile A

Carburized layer hardness gradient measurement is a precision microhardness testing technique that maps the hardness profile from the hardened case to the core of carburized steel components, verifying effective case depth and heat treatment quality. Performed in accordance with ISO 2639, GB/T 9450, ASTM E384 and related standards, this test is essential for validating gears, bearings and shafts whose fatigue life and wear resistance depend directly on case depth and gradient steepness. Accredited third-party laboratories provide traceable hardness gradient data that supports process qualification, product validation and failure analysis.

Technical Overview

Carburizing is a thermochemical heat treatment in which carbon is diffused into the surface of a low-carbon steel at approximately 880–950 °C, followed by quenching and low-temperature tempering. The result is a high-carbon, high-hardness martensitic case over a tough, low-carbon core, which is the combination required by heavily loaded components such as gears, bearings and shafts. Because part performance is governed not by surface hardness alone but by the entire hardness profile, the carburized layer hardness gradient measurement has become the primary acceptance test for carburized parts.

The test is performed on a polished cross-section using a microindentation traverse, typically with a Vickers indenter under HV0.5 to HV1 loads. Hardness values are plotted against distance from the treated surface to construct the gradient curve, from which several key parameters are extracted: surface hardness, effective case depth (DC or CHD), total case depth, core hardness and the steepness of the transition zone. According to ISO 2639, GB/T 9450 and DIN 50190-1, the effective case depth is defined as the depth at which the hardness equals 550 HV1 (approximately 52 HRC), while SAE and common North American practice often specifies the depth at 50 HRC (approximately 513 HV).

The measurement chain relies on recognized international and national standards, including ISO 2639 and GB/T 9450 for effective case depth determination, GB/T 9451 for total hardening depth, SAE J423 for case depth test methods, ISO 6507 and ASTM E384 for Vickers and microindentation hardness testing, and ASTM E140 / ISO 18265 for hardness value conversions. Accredited third-party laboratories operating under ISO/IEC 17025 quality systems combine these methods with calibrated instrumentation to deliver traceable, repeatable case depth results.

Testing Samples

Gear Teeth and Transmission Components

Transverse sections cut through the mid-height of gear teeth are the most frequently tested carburized samples. For automotive passenger car gears, effective case depth requirements typically fall in the 0.6–1.2 mm range, while commercial vehicle, off-highway and wind turbine gears may require 1.5–4 mm or more. A common design rule of thumb relates effective case depth to gear module, generally 0.15–0.25 times the module, and the measured gradient must confirm that the specified depth is achieved without case-core interface weaknesses.

Bearing Rings, Rollers and Races

Case-carburized bearing components made from grades such as SAE 8620, 20CrMo, 20CrMnTi and 18CrNiMo7-6 are sectioned radially or transversely through the raceway or rolling contact surface. Deep case bearings may require effective case depths exceeding 3 mm to resist subsurface contact fatigue, so the hardness traverse must extend well into the core to fully document the transition behavior.

Shafts, Splines and Constant-Velocity Joints

Camshafts, crankshafts, output shafts, spline sections, tripod and ball-type constant-velocity joint housings are sampled at the most functionally critical locations, such as fillets, tooth flanks and ball tracks. Where a single part has multiple carburized surfaces with different depth specifications, each surface is sectioned and tested separately.

Pins, Fasteners and Small Cross-Sections

Small parts including rollers, needles, pins, bushings and fasteners can often be mounted whole for cross-sectional testing. For these shallow cases, reduced indentation forces (HV0.1 to HV0.5, or Knoop indentation per ASTM E384) are applied so that the plastic zone of each indentation remains well inside the case layer and does not interact with the underlying core.

Specimen Preparation Requirements

Samples must be sectioned perpendicular to the treated surface using abrasive cutting under flood coolant to avoid burning or re-tempering the case. Edge retention during mounting, grinding and polishing is critical; the surface layer must remain perfectly flat and undamaged to the very edge. Final polishing to 1 µm diamond or finer, optionally followed by a light 2–3% nital etch to reveal the case microstructure, prepares the specimen for accurate microhardness measurement.

Testing Items

A complete carburized layer hardness gradient evaluation typically reports the following measurable items:

  • Surface hardness (converted to HRC or reported directly in HV)
  • Effective case depth (DC) at the 550 HV1 limit hardness per ISO 2639 / GB/T 9450, or at 50 HRC where specified
  • Total case depth determined by hardness plateau analysis per GB/T 9451
  • Core hardness measured beyond the case-core transition
  • Tabulated hardness versus depth data and the plotted hardness gradient curve
  • Depths at multiple intermediate limit values, for example 700 HV, 600 HV, 550 HV and 500 HV
  • Gradient steepness and transition zone characterization
  • Detection of anomalies such as surface softening from decarburization or excessive retained austenite, and sub-surface hardness dips from carbide banding or non-martensitic transformation products
  • Hardness conversions between HV, HRC and HK reported per ASTM E140 / ISO 18265 for information

Testing Methods

Microindentation Traverse Procedure

A Vickers microhardness traverse is the reference method. Indentations are placed along a line normal to the carburized surface, with the first indentation as close to the surface as edge-effect rules permit. In accordance with ISO 6507-1, the distance between the centers of adjacent indentations must be at least 2.5 times the indentation diagonal, and for effective case depth determination the depth increment between measuring points is typically held to 0.1 mm or less to achieve adequate resolution. Where additional confidence is required, two parallel traverse rows offset laterally by at least 2.5 diagonals are measured and averaged.

Gradient Curve Evaluation and Effective Case Depth Determination

The measured hardness values are plotted against distance from the surface, and a smooth best-fit curve is drawn through the data points. The effective case depth is the depth coordinate at which this curve intersects the specified limit hardness, normally 550 HV1, determined by interpolation between the two adjacent data points that bracket the limit. Depths at alternative limit hardness values are read from the same curve on request, providing a complete quantitative description of the case.

Two-Point Verification Method

For routine verification of a specified case depth, as described in ISO 2639 and GB/T 9450, indentation pairs are placed just inside and just outside the specified depth position. If the nearer-surface indentation exceeds the limit hardness and the deeper indentation falls below it, the effective case depth is confirmed to coincide with the drawing requirement, and the interpolated depth between the two points is reported. This method substantially reduces testing time for series inspection.

Supplementary Macro-Hardness Methods

For very deep cases, HV5 or HV10 indentations, or Rockwell C testing on step-ground or tapered specimens per SAE J423, may be used as a coarser alternative. Knoop microindentation per ASTM E384 is preferred for very shallow hardened layers where Vickers diagonals would be unacceptably large relative to the case thickness. All conversion between scales is performed per ASTM E140 / ISO 18265 and clearly identified as converted data.

Equipment Calibration and Quality Control

Testing is conducted with microhardness testers verified in accordance with ISO 6507-2 and ASTM E384, using certified reference blocks traceable to national metrology institutes. Optical measuring systems are calibrated for diagonal reading, and laboratories report typical case depth measurement uncertainties on the order of ±0.03–0.05 mm, depending on gradient steepness and indentation spacing. Test reports identify the applicable standard, test force, indentation spacing, measured data table, gradient curve and all assumed conversion relationships.

Applications

Carburized layer hardness gradient measurement is applied across every industry that relies on case-hardened steel components, supporting design validation, heat treatment process control, supplier qualification and root-cause failure investigation. Typical applications include:

  • Automotive transmission and final-drive gear development, process sign-off and serial production audits
  • Wind turbine and industrial gearbox gears requiring thick, carefully controlled cases
  • Case-carburized bearing rings, rollers and races for rolling contact fatigue resistance
  • Aerospace actuator gears and engine components processed to SAE AMS carburizing specifications
  • Rail, construction machinery, agricultural equipment and oilfield power-transmission components
  • Heat treatment process qualification, carbon potential and cycle-time optimization studies
  • Failure analysis of spalling, case crushing, tooth breakage and subsurface fatigue, where the measured gradient is compared against design intent to identify under-carburizing, over-tempering or excessive retained austenite
  • Incoming inspection and material qualification of carburizing steel grades such as SAE 8620, 20CrMnTi, 20CrNiMo and 18CrNiMo7-6

FAQ

What defines the effective case depth of a carburized part?

Effective case depth is the distance from the hardened surface to the depth at which hardness equals 550 HV1 (approximately 52 HRC) under ISO 2639, GB/T 9450 and DIN 50190-1. Some specifications, particularly in North American SAE practice, instead use 50 HRC, which corresponds to approximately 513 HV. The applicable criterion should always be stated explicitly on the engineering drawing to avoid ambiguity.

What is the difference between effective case depth and total case depth?

Effective case depth marks the location of a functional hardness limit that correlates with load-bearing capacity, while total case depth is the distance to the point where hardness becomes indistinguishable from the core, determined either by hardness plateau analysis per GB/T 9451 or by microstructural examination. Total case depth is always equal to or greater than effective case depth, typically by 0.2–0.5 mm or more depending on steel hardenability.

Which indentation load should be used for the hardness traverse?

HV1 (9.807 N) is the preferred load for carburized cases of roughly 0.3 mm effective depth and above, because the diagonal remains small relative to the case thickness. For shallower cases, HV0.5 or lower forces, or Knoop indentation with elongated indentations, provide better spatial resolution. The governing principle is that indentation size and spacing must not allow the core or neighboring indentations to influence the measured hardness values.

How close to the surface can the first hardness measurement be made?

The first indentation is placed as close to the surface as possible while respecting the minimum edge distance of approximately 2.5 times the indentation diagonal, so that the edge does not distort the indentation. Surface hardness itself is often verified independently by Rockwell C testing per ASTM E18 on the functional surface, complementing the cross-sectional gradient data.

Can the hardness gradient test be performed non-destructively?

No. Cross-sectional microhardness traverse is inherently destructive because the component must be cut, mounted and polished. Step-grinding methods per SAE J423 are semi-destructive alternatives for deep cases, while portable hardness testing can only approximate surface hardness and cannot resolve the case depth or gradient. Destructive testing is therefore performed on sacrificial witness coupons processed together with production parts where components must remain intact.

Why is surface hardness sometimes lower than the peak hardness just beneath it?

This common gradient feature usually reflects excessive surface carbon producing retained austenite, or slight surface decarburization, oxidation or transformation products from the heat treatment atmosphere. Because final grinding removes some case material, specifications often allow the peak hardness to sit slightly below the surface; however, severe surface softening reduces wear and fatigue performance and should be investigated.

What sample size and turnaround are typical for this test?

A representative section of the component, often a single gear tooth segment or a ring slice 10–20 mm across, is sufficient. Standard turnaround for sectioning, mounting, polishing, microhardness traverse, curve analysis and formal reporting at an accredited third-party laboratory is typically three to five working days, with expedited services available for production-critical or failure analysis projects.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing