Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Air Content Testing of Fresh Concrete Mixtures: Methods, Standards, and Technical Requirements

Air content testing of fresh concrete mixtures is a fundamental quality control procedure that measures the total volume of entrained and entrapped air in concrete before placement, providing a direct indicator of freeze-thaw durability, workability, and long-term structural performance. This technical guide covers the testing principle, sampling requirements, primary test methods under standards such as ASTM C231, ASTM C173, EN 12350-7, and GB/T 50080, and the typical engineering applications of air content determination.

Technical Overview

Air content testing of fresh concrete mixtures (fresh concrete air content determination) quantifies the volume percentage of air voids present in freshly mixed, unhardened concrete. Concrete contains two distinct categories of air voids: entrapped air, which is unintentionally captured during mixing and typically accounts for 1% to 2% of volume, and entrained air, which is deliberately introduced through air-entraining admixtures conforming to ASTM C260 to create a stable system of microscopic bubbles typically ranging from 10 to 500 micrometers in diameter.

Entrained air voids serve as relief chambers within the cement paste. When moisture inside hardened concrete freezes, the expanding water is forced into these tiny bubbles, relieving hydraulic pressure that would otherwise cause internal cracking and progressive deterioration. For this reason, building codes such as ACI 318 and specifications including ACI 301 mandate minimum air contents for concrete exposed to freeze-thaw cycles or de-icing chemicals. Beyond durability, entrained air also improves workability, reduces bleeding and segregation, and enhances cohesion in mixtures with harsh or poorly graded aggregates.

Because air content has a direct trade-off with compressive strength (a strength reduction of approximately 2% to 6% is commonly attributed to each 1% increase in air content), it must be controlled within a specified tolerance band, generally 4% to 8% depending on exposure class and nominal maximum aggregate size. Field verification of air content in the fresh state is therefore a routine acceptance test at batching plants, during transport, and at the point of placement. The governing international and national standards include ASTM C231/C231M, ASTM C173/C173M, ASTM C138/C138M, EN 12350-6, EN 12350-7, and GB/T 50080.

Testing Samples

Sampling Location and Procedure

Representative samples of fresh concrete shall be obtained in accordance with ASTM C172, EN 12350-1, or GB/T 50080. For revolving-drum truck mixers, sampling should be taken from the middle portion of the discharge, discarding the first and last approximately 10% to 15% of the load, unless the entire discharge is being evaluated. Samples from stationary mixers, paving mixers, or agitators shall be taken at two or more evenly spaced points during discharge and combined into a composite sample.

Sample Volume and Handling

  • The minimum sample volume should be approximately 0.03 cubic meters (1 cubic foot), or at least 1.25 times the volume required to fill the measuring vessel of the air meter with excess for strike-off.
  • Testing shall commence within approximately 5 minutes of obtaining the sample, as delayed testing can allow measurable air loss or continued hydration to alter results.
  • Samples must be protected from rapid moisture loss, contamination, vibration, and temperature extremes during transport to the test location.
  • Concrete temperature shall be recorded at the time of sampling, since air content measurement is temperature-sensitive and specifications frequently limit placement between roughly 5 degrees Celsius and 35 degrees Celsius.

Testing Items

The core measured parameter is the air content of the fresh concrete sample, expressed as a percentage of the total volume of the concrete. Depending on the selected method, the following related determinations are performed or reported:

  • Total air content of fresh concrete (percentage by volume of concrete).
  • Aggregate correction factor, determined for pressure methods to account for air contained within the aggregate particles themselves.
  • Fresh concrete density (unit weight), yield, and gravimetric air content, determined together under ASTM C138 or the density method of GB/T 50080.
  • Supporting fresh-state properties typically measured on the same sample, including slump or flow in accordance with ASTM C143 or EN 12350-8, and concrete temperature.

Testing Methods

Pressure Method (ASTM C231, EN 12350-7, GB/T 50080)

The pressure method is the most widely used procedure for normal-weight concrete. The apparatus consists of a calibrated measuring bowl and a sealed air chamber connected through a valve, employing either a Type A (column of water) or Type B (pressure gauge) meter. The principle is based on Boyle's law: a known pressure is applied to the concrete sample, and the observed pressure drop or water-level change at equilibrium corresponds to the volume of air compressed within the mortar fraction of the concrete.

  • The bowl is filled in layers, each consolidated by 25 strokes of rodding or by internal vibration, followed by tapping of the vessel exterior to release trapped air pockets.
  • The surface is struck off level, the cover assembly is clamped water-tight, and water or pressure is introduced through the operating valves.
  • Pressure is applied to the calibrated value, the meter is tapped and rocked gently, and the air content is read directly from the gauge or meniscus column.
  • An aggregate correction factor, obtained separately by testing the saturated aggregate in water, must be subtracted from the indicated reading to obtain the true air content of the concrete.
  • The pressure method is not applicable to concrete containing lightweight aggregates, cellular concrete, or highly porous materials whose air voids do not respond to applied pressure in the same manner as the mortar air system.

Volumetric Method (ASTM C173, GB/T 50080)

The volumetric method, often performed with a roll-about type apparatus, determines air content by direct volume displacement. The measuring bowl is filled and consolidated as in the pressure method, after which a calibrated neck is topped with water, and the sealed unit is rolled and agitated until the air in the sample has been displaced by water. Isopropyl alcohol is frequently used as a foaming control agent. The drop of the water level in the graduated neck, corrected per the calibration of the apparatus, indicates the air content. This method is the preferred choice for lightweight and porous-aggregate concretes because it does not rely on aggregate compressibility assumptions.

Gravimetric Method (ASTM C138, GB/T 50080)

The gravimetric (density) method calculates air content by comparing the theoretical density of a fully compacted, air-free mixture with the actual measured density of the fresh concrete. The sample is consolidated by rodding or vibration into a calibrated container of known volume, weighed, and the actual density computed. Air content is then determined as the difference between theoretical and actual densities divided by the theoretical density, expressed as a percentage. This method requires accurate and complete batch proportions and is most reliable as a plant-level verification tool.

Super Air Meter (SAM) and Advanced Evaluation

The Super Air Meter is an extension of the Type B pressure meter that applies a sequence of pressure steps to estimate both total air content and the SAM number, an index correlating with the air-void spacing factor in hardened concrete. It is increasingly used as a rapid field screening tool to assess not only how much air is present, but whether the air-void system is likely to provide adequate freeze-thaw protection, supplementing hardened concrete air-void analysis under ASTM C457.

Applications

Air content testing is applied across virtually every sector where concrete durability is governed by exposure conditions:

  • Freeze-thaw exposed infrastructure such as bridge decks, highway pavements, airport runways, and parking structures subject to de-icing salts.
  • Marine and hydraulic structures including ports, breakwaters, dams, and spillways exposed to wetting-drying and freezing cycles.
  • Ready-mixed concrete production control, verifying air-entraining admixture dosing and compensating for the effects of supplementary cementitious materials, chemical admixtures, and cement fineness on air stability.
  • Pumped concrete and long-haul deliveries, where air loss during handling, pumping, and prolonged agitation must be quantified to ensure placement within specification limits.
  • Winter concreting programs and mass concrete works where entrained air improves resistance to early-age thermal and frost damage.
  • Acceptance testing and dispute resolution between contractors, suppliers, and owners, with tests performed by accredited third-party laboratories or certified field technicians.

FAQ

What is the typical specified air content range for air-entrained concrete? Most specifications require 4% to 8% total air content, with the exact target depending on the exposure class (mild, moderate, or severe freeze-thaw) and the nominal maximum aggregate size. Larger aggregates require lower target air contents because less mortar paste is present per unit volume of concrete.

Why must an aggregate correction factor be applied in the pressure method? Natural aggregates contain internal pores that hold air which is compressed during pressurization but does not contribute to the protective air-void system in the paste. Without subtracting this factor, the indicated reading overstates the true air content of the concrete.

Which method should be used for lightweight concrete? The volumetric method (ASTM C173) should be used, because porous lightweight aggregates distort pressure-based readings and invalidate the assumptions of the pressure method.

How does air content affect concrete strength? Each 1% increase in air content generally reduces compressive strength by approximately 2% to 6%. This strength penalty is the principal reason air content must be kept within the specified tolerance rather than maximized.

How frequently should air content be tested on a project? Typical specifications require testing on the first truck of each day, at regular intervals such as every 100 to 150 cubic meters placed, whenever mix materials or admixture dosages change, and whenever any indication of abnormal workability or finishability is observed.

What causes air loss between the plant and the point of placement? Excessive mixer revolution counts, prolonged agitation, elevated concrete temperature, over-vibration, high pumping pressures, and interactions between air-entraining admixtures and certain water reducers or supplementary cementitious materials can all reduce air content. Measuring air content at both the plant and the placement point is a common diagnostic practice.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing